MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chevron Phillips Marlex® 5104 LDPE Blow Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Blow Molding Grade

Material Notes: This autoclave, low density, ethylene homopolymer is tailored for blow molded applications that require:
  • Good impact resistance
  • Excellent flexibility
  • Good clarity
  • Good gloss
  • No slip or antiblock
Typical blow molded applications for 5104 include:
  • Pharmaceutical bottles
  • Squeeze bottles
  • Flexible toys
Typical extrusion applications for 5104 include:
  • Wood-plastic composite component
  • Blends to improve friction values
  • Blends to enhance part flexibility
  • Adhesives
This resin meets these specifications:
  • ASTM D4976 - PE 113
  • FDA 21 CFR 177.1520(c) 2.2, use conditions B through H per Table 2 of 21 CFR 176.170(c)
  • Listed in the Drug Master File

Data provided by Chevron Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.924 g/ccASTM D1505
Melt Flow 1.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 16.0 MPa2 in/min, Type IV bar; ASTM D638
Elongation at Break 600 %2 in/min, Type IV bar; ASTM D638
Flexural Modulus 0.340 GPaTangent - 16:1 span:depth, 0.5 in/min; ASTM D790
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -75.0 °CType A, Type I specimen; ASTM D746
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade
Dow LDPE 5004I Low Density Polyethylene, Extrusion Coating Grade
Amco PRIMATOP LDPE 023919 Blow Molding Polyethylene
Chevron Phillips Marlex® 1122B Injection Molding Resin
Chevron Phillips Marlex® 4538A LDPE Blow Molding Resin

PCHEVV84 / 20480

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.