  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

TechnoCompound TechnoDur PBT/PET GF 20 Natural (9969) PBT/PET, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + PET Blend, Glass Filled

Material Notes: Our new TechnoDur PBT compound is a thermoplastic which combines great hardness, stiffness and strength. TechnoDur is easily processed due to its perfect flow behavior. The favorable sliding and wear characteristics as well as extremely high tenacity in temperatures below freezing are further advantages.

Typical Applications: TechnoDur compounds may be applied in the following areas:

  • Electrical engineering: Lamp holders, micro switches, spools, brush-holder bridges, switches, cam devices, telephone housings
  • Automobile construction: Junction boxes, petrol filters, fuel tank caps, heating, folds, headlights, car body panels, spark plug connectors
  • Household appliances: Hair care appliances, components for toasters, fondue makers, coffeemakers
  • Other: pump components, gears guide applications: slide bearings and components

Information provided by TechnoCompound

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.47 g/cc0.0531 lb/in³ISO 1183
Moisture Absorption 0.200 %
@Time 86400 sec
0.200 %
@Time 24.0 hour
ISO 62
Water Absorption at Saturation 0.40 %0.40 %ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm
@Pressure 60.0 MPa,
Temperature 260 °C
0.0030 in/in
@Pressure 8700 psi,
Temperature 500 °F
WZ 80 °C; ISO 2577
Linear Mold Shrinkage, Transverse 0.010 cm/cm
@Pressure 60.0 MPa,
Temperature 260 °C
0.010 in/in
@Pressure 8700 psi,
Temperature 500 °F
WZ 80 °C; ISO 2577
Melt Flow 18 g/10 min
@Load 0.00216 kg,
Temperature 265 °C
18 g/10 min
@Load 0.00476 lb,
Temperature 509 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 200 MPa
@Load 36.5 kg
29000 psi
@Load 80.5 lb
ISO 2039-1
Tensile Strength at Break 135 MPa19600 psi5 mm/min; ISO 527
Elongation at Break 3.0 %3.0 %5 mm/min; ISO 527
Tensile Modulus 7.80 GPa1130 ksi1 mm/min; ISO 527
Flexural Strength 195 MPa28300 psi2 mm/min; ISO 178
 195 MPa
@Strain 3.5 %
28300 psi
@Strain 3.5 %
2 mm/min; ISO 178
Flexural Modulus 6.20 GPa899 ksi2 mm/min; ISO 178
Flexural Strain at Break 3.5 %3.5 %2 mm/min, flexural strength; ISO 178
Charpy Impact Unnotched  4.00 J/cm²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
 4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
Charpy Impact, Notched  0.900 J/cm²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eA
 0.900 J/cm²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Constant  3.6
@Frequency 1e+6 Hz
3.6
@Frequency 1e+6 Hz
IEC 60251
 3.8
@Frequency 100 Hz
3.8
@Frequency 100 Hz
IEC 60250
Dielectric Strength 26.0 kV/mm
@Thickness 1.00 mm
660 kV/in
@Thickness 0.0394 in
Short Time; IEC 60243-1
Comparative Tracking Index 250 V250 VA; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 40.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
22.2 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
38.9 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359
Melting Point 220 - 255 °C428 - 491 °FISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °FISO 75
Deflection Temperature at 8.0 MPa 95.0 °C203 °FISO 75
Vicat Softening Point 210 °C
@Load 5.10 kg
410 °F
@Load 11.2 lb
50 °C/h; ISO 306
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
Glow Wire Flammability Index 750 °C
@Thickness 2.00 mm
1380 °F
@Thickness 0.0787 in
IEC 60695-2-12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTECHNO031 / 306393

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.