MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Shingle Oil
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Shingle Oil is a straw colored, low viscosity oil designed for use as a shingle or shake dressing for shake roofs, wooden fencing, wood siding, and log homes.

Chevron Shingle Oil penetrates the wood surface to enhance or replace natural oils and resins leached out by cyclical exposure to sun and rain. Although Chevron Shingle Oil retards the aging process, it will not renew wood that is already weather damaged.

Applications

Loose dirt and debris should be removed before the oil is applied. The roof should be hosed with water 24 hours prior to application to lessen the possibility of over application. Alternatively, a licensed contractor can power wash the roof thereby removing weatherdamaged wood, allowing oil to absorb into new wood.

Chevron Shingle Oil may be applied by brushing or spraying. The typical application rate is 150-300 square feet per gallon. Application rate depends on the type of wood and the rate at which the oil saturates the wood.

Do not overapply — Over application may lead to shingle or shake "cupping" and the presence of oil in rainwater runoff.

Do not add color pigments — as they will lump and settle out.

Do not walk on treated surfaces — Chevron Shingle Oil is a petroleum oil and is slippery.

Do not use on flat surfaces, such as decks. Properly licensed contractors may add certain chemicals, such as antifungal agents and other substances, to Chevron Shingle Oil. Be sure to find out what safety or health restrictions may apply to these additives.

Key Words: CPS Number: 213304; MSDS Number: 4223
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 23.4 °
Volatile Organic Compounds (VOC) Content 130 g/l
Kinematic Viscosity at 40°C (104°F) 21.7 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 3.5 cStASTM D445
 
Thermal PropertiesOriginal ValueComments
Pour Point -42.0 °CASTM D97
Flash Point 183 °CASTM D92
 
Descriptive Properties
Color0.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chi Mei Polyrex® PH-888G Polystyrene - High gloss
KKPC KOSYN KTR 101 Thermoplastic Elastomer (TPE)
Elkem (Bluestar Silicones) SILCOLAPSE® 426R Silicone Emulsion
Covestro Bayblock® Base GS Acrylic Basecoat
American Red Western Cedar (Giant Arborvitae) Wood

WCHEV357 / 74972

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.