MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Malleable iron casting, Class 35018
Categories: Metal; Ferrous Metal; Cast Iron; Malleable Iron

Material Notes: Temper carbon and ferrite microstructure. Applications include general engineering service at normal and elevated temperatures for good machinability and excellent shock resistance.

Key Words: ASTM A47, ASTM A338, ANSI G48.1, FED QQ-I-666c, Malleable iron casting grade 35018, ferritic, good machinability, shock resistant
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell <= 156
Hardness, Knoop 173Estimated from Brinell
Hardness, Vickers 161Estimated from Brinell
Tensile Strength, Ultimate 365 MPa
Tensile Strength, Yield 241 MPa
Elongation at Break 18 %
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 2.0 - 2.45 %
Iron, Fe 96 %
Manganese, Mn 0.25 - 0.55 %
Phosphorus, P <= 0.050 %
Silicon, Si 1.0 - 1.35 %
Sulfur, S 0.030 - 0.18 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Malleable iron casting, Class 32510
ASTM A197 malleable iron casting
Ductile Iron grade 60-40-18
Malleable iron casting, Class 40010
ASTM class 30 Standard gray iron test bars, as cast

MMFE02 / 12424

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.