MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilamid® LVX-65H SST black 9288 PA12-GF65
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 50% Glass Fiber Filled

Material Notes: Product description: Grilamid LVX-65H SST black 9288 is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following product profile:
  • Very high stiffness and strength
  • Excellent impact and notched impact strength
  • Excellent UV, heat and chemical resistance
  • Very low moisture absorption
  • Suitable for often repeated steam sterilization
  • Good flow characteristics
  • High molding precision, low warpage
Grilamid LVX-65H SST black 9288 is suitable for production of technical parts in applications such as:
  • Housings of electronic devices
  • Automotive
  • Mechanical engineering
  • Safety components
  • Housings of medical devices and instruments

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.70 g/ccDry; ISO 1183
Water Absorption 0.80 %Sim. to ISO 62
Moisture Absorption 0.400 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0030 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 190 MPaConditioned; ISO 2039-1
 210 MPaDry; ISO 2039-1
Tensile Strength at Break 185 MPaConditioned; ISO 527-1/-2
 200 MPaDry; ISO 527-1/-2
Elongation at Break 2.5 %Dry; ISO 527-1/-2
 2.5 %Conditioned; ISO 527-1/-2
Tensile Modulus 17000 MPaConditioned; ISO 527-1/-2
 19000 MPaDry; ISO 527-1/-2
Charpy Impact Unnotched 80.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eU
 80.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 85.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eU
 85.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 20.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 20.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 20.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 20.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Strength 35.0 kV/mmDry; IEC 60243-1
 35.0 kV/mmConditioned; IEC 60243-1
Comparative Tracking Index 600 VConditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 10.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 70.0 µm/m-°CISO 11359-1/-2
Melting Point 178 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 120 °CLong Term; ISO 2578
 150 °CShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 175 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 160 °CISO 75-1/-2
 
Descriptive Properties
AutomotiveAutomotive electr. and electronics, lighting
 Compressed air systems
 Hydraulic systems
 Powertrain and Chassis
Electricals & ElectronicsConnectors
 Electrical appliances
 Electrical equipment
 Mobile phones and other portable devices
FormGranules
Industry & Consumer goodsHousewares
 Hydraulics & Pneumatics
 Mechanical Engineering
 Medical devices
 Power transmission
 Sanitary, water and gas supply
 Sports & Leisure
 Tools & Accessories
ProcessingInjection Molding
Product AttributesImproved flowability and demolding
Special CharacteristicsHigh impact or impact modified
 Improved heat resistance
 Improved UV resistance (outdoor use)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® LBV-65H FWA black 9225 PA12-GF65
EMS-Grivory Grilamid® LV-65H FWA black 9225 PA12-GF65
EMS-Grivory Grilamid® LV-65H SST black 9288 PA12-GF65
Covestro Makrolon® 2558 Polycarbonate
EnviroBrass® (SeBiLOY®) III Lead-Free Yellow Brass Casting Alloy, UNS C89550

PGRH092 / 156801

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.