MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Matexcel CER-0060 Mica Gaskets
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Mica Gaskets have a flexible texture & elasticity, and an outstanding performance as high thermal insulation. Mica Gaskets resist operating temperatures up to 1800°F Applications include but not limited to: Supports for heating resistors (i.e. convectors). Thermal insulation in circuit breakers and between electronic components In large thickness, as thermal insulators for industries with large stress such as iron and steel works, chemical, glass and petro-chemical industries Mechanical support and electrical insulator in high voltage cabins Replacements for asbestos panels in forging machines and hydraulic presses Automotive (exhaust manifolds) Fuel cells; gas turbines & turbo generators. It can also be used as filler for spiral wound gaskets or as a material for cam profile gaskets.

Mica Gaskets

Key Words: Synonyms: Mica Gaskets
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size 100 - 250 µmrolls
 100 - 3000 µmsheets
 
Descriptive Properties
ComponentsMica Gasket is made from high-grade Phlogopite mica paper impregnated with a silicone binder. Phlogopite mica (= aluminosilicate of mineral origin) gives AX-TEMP it´s thermal characteristics & outstanding resistance to solvents, acids and mineral oils.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMXCK1497 / 300128

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.