MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Sultron™ LSG PPSU Extruded, Unfilled, Polyphenylsulfone (ASTM Product Data Sheet)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: Sultron™ Life Science Grade (LSG) Polyphenylsulfone PPSU biocompatible shapes offer superior hydrolysis resistance as measured by steam autoclaving cycles, making them an excellent choice for medical device applications. Sultron™ LSG PPSU components also resist common acids and bases, including commercial washing solutions, over a broad temperature range. Often favored across the medical and life sciences industry for their wide array of color options, Sultron™ LSG PPSU components can be found in sterilization trays, dental and surgical instrument handles, and in fluid handling coupling and fitting applications.

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Key Words: formerly Sultron™ LSG PPSU R5500
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.29 g/ccASTM D792
Water Absorption 0.37 %24 hour immersion; ASTM D570
Water Absorption at Saturation 1.1 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 80ASTM D785
Hardness, Rockwell R 120ASTM D785
Hardness, Shore D 80ASTM D2240
Tensile Strength 11000 psiASTM D638
Tensile Strength at 150°C (300°F) 5000 psiASTM D638
Tensile Strength at 65°C (150°F) 8000 psiASTM D638
Elongation at Break 30 %ASTM D638
Tensile Modulus 339 ksiASTM D638
Flexural Strength 15500 psiASTM D790
Flexural Modulus 345 ksiASTM D790
Compressive Yield Strength 13400 psi10% deformation; ASTM D695
Compressive Modulus 280000 psiASTM D695
Shear Strength 9.00 ksiASTM D732
Izod Impact, Notched 2.50 ft-lb/inASTM D256
K (wear) Factor >= 1000 x 10-10 in³-min/ft-lb-hrQTM 55010
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square >= 1.00e+13 ohmEOS/ESD S11.11
Dielectric Constant 3.44
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 360 V/milASTM D149
Dissipation Factor 0.0017
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 31.0 µin/in-°F
@Temperature -40.0 - 149 °C
ASTM E831
Thermal Conductivity 2.42 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 340 °F
Deflection Temperature at 1.8 MPa (264 psi) 405 °FASTM D648
Glass Transition Temp, Tg 428 °FASTM D3418
Flammability, UL94 V-0
@Thickness 3.10 mm
 
Compliance PropertiesOriginal ValueComments
3A-Dairy No
Canada AG No
FDA Yes
NSF No
USDA No
USP Class VI Yes
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Limited
Acids, Weak Acceptable
Alcohols Limited
Alkalies, Strong (pH 11-14) Acceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Unacceptable
Conductive / Static Dissipative No
Continuous Sunlight Limited
Hot Water / Steam Acceptable
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Limited
Inorganic Salt Solutions Acceptable
Ketones, Esters Unacceptable
 
Descriptive Properties
Colorvarious

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Ketron™ 1000 PEEK, Extruded Unfilled Polyetherether Ketone
BASF Ultrason® P 3010 PPSU Unreinforced Polyphenylsulfone
Mitsubishi Chemical Advanced Materials Sultron™ PSU Extruded Unfilled Polysulfone
Overview of materials for Polyphenylsulfone (PPSU)
Ensinger RADEL® R-5500 Polyphenylsulfone (PPSU)

P1SM27E / 129698

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.