MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Borealis Queo™ 0230 Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Queo 0230 is an ethylene based octene-1 plastomer, produced in a solution polymerization process using a metallocene catalyst. CAS-No. 26221-73-8

Special Features:

  • Versatile blending with other polyolefins in film, extrusion and molding applications
  • Outstanding toughness
  • Outstanding puncture resistance
  • Low temperature impact strength
  • High flexibility and surface softness
  • High clarity
  • Excellent low-temperature flex-cracking resistance
  • High filler and oil acceptance
Applications:
  • Carpet backing
  • Powder coating
  • Color master batches
  • Highly filled compounds
  • Extrusion coating
Additives: Queo 0230 contains a low amount of processing stabilizers

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.902 g/cc0.0326 lb/in³ISO 1183
Viscosity  30.0 cP
@Shear Rate 10000 1/s,
Temperature 230 °C
30.0 cP
@Shear Rate 10000 1/s,
Temperature 446 °F
DIN 54811
 90.0 cP
@Shear Rate 100 1/s,
Temperature 230 °C
90.0 cP
@Shear Rate 100 1/s,
Temperature 446 °F
DIN 54811
 100 cP
@Shear Rate 1000 1/s,
Temperature 190 °C
100 cP
@Shear Rate 1000 1/s,
Temperature 374 °F
DIN 54811
 400 cP
@Shear Rate 10000 1/s,
Temperature 190 °C
400 cP
@Shear Rate 10000 1/s,
Temperature 374 °F
DIN 54811
Environmental Stress Crack Resistance <= 120 hour<= 120 hourASTM D 1693-B
Melt Flow 30.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
30.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 38.038.0ISO 868
Tensile Strength 11.0 MPa1600 psiISO 527-2
Elongation at Break 875 %875 %ISO 527-2
Flexural Modulus 0.0650 GPa9.43 ksiISO 178
Izod Impact, Notched (ISO) NBNBISO 180/1A
 
Thermal PropertiesMetricEnglishComments
Melting Point 97.0 °C207 °FISO 11357-3
Vicat Softening Point 71.0 °C
@Load 1.02 kg
160 °F
@Load 2.25 lb
ISO 306
Brittleness Temperature <= -90.0 °C<= -130 °FASTM D 746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBORE9891 / 323248

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.