MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Covestro MULTRANOL® 9190 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Multranol 9190 is a 4,000-molecular-weight polypropylene oxide-based diol.

Properties / Applications: Multranol 9190 is a 4,000 molecular-weight polypropylene oxide-based diol specially modified with ethylene oxide. It is used in the production of solid and microcellular urethane elastomers. As with any product, use of Multranol 9190 polyol in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.015 g/cc
@Temperature 60.0 °C
 1.02 g/cc
@Temperature 25.0 °C
 1.03 g/cc
@Temperature 40.0 °C
Bulk Density 63.7 lb/ft³
Viscosity 400 cP
@Temperature 45.0 °C
 700 cP
@Temperature 30.0 °C
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.050[mg KOH/g]
 
Thermal PropertiesOriginal ValueComments
Flash Point 287 °CPMCC
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.050 %
 
Descriptive Properties
AppearanceClear to slightly hazy liquid
Color<100APHA
Hydroxyl number[mg KOH/g]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Axiall 9190 Rigid PVC, Molding

PCOVEST0948 / 202731

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.