MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Parker Chomerics CHO-SHIELD® 2001 Conductive Coating
Categories: Polymer; Adhesive; Thermoset

Material Notes: Electrically conductive coatings provide corrosion protection for enclosure flanges which mate with EMI shielding gaskets. They can also provide a corrosion resistant conductive surface coating on aluminum or non-conductive composite substrates.CHO-SHIELD 2001 coating is light brown. It contains soluble chromate salts that minimize the effects of galvanic corrosion of the aluminum substrate, even in the event of a coating scratch.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 3.10 g/cc3.10 g/cc
Volatile Organic Compounds (VOC) Content 554 g/l554 g/l
Thickness 76.2 microns3.00 milRecommended
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square <= 0.10 ohm<= 0.10 ohm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 85.0 °C185 °F
Minimum Service Temperature, Air -65.0 °C-85.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 min
@Temperature 24.0 °C
2.00 hour
@Temperature 75.2 °F
followed by 30 min. at 121°C
 10100 min
@Temperature 24.0 °C
168 hour
@Temperature 75.2 °F
Working Life 120 min120 min
Shelf Life 9.00 Month9.00 Month
 
Descriptive Properties
BinderUrethane
ColorLight Brown
ConsistencyMedium Fluid
Coverage 40 ft2/qt
FillerCu, Soluble Chromate salts
Mix RatioPre-measured kit
Suggested Spraying19 - 27 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHOME168 / 28390

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.