MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

China Tungsten YT14 Tungsten Carbide for Cutting Tools
Categories: Ceramic; Carbide

Material Notes: High strength in use and good impact & shock resistance, yet lower than YT5,Rough turning and rough milling of carbon steel and alloy steel during continuous cutting or medium to fine turning of them during intermittent cutting

Information provided by China Tungsten

Key Words: ISO P20
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 11.4 g/cc0.412 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell A 91.591.5
Flexural Strength 1750 MPa254000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Crucible Steel CSM® 2 Mold Steel, AISI P20
EDRO #3 Prehardened Mold Quality P20 Alloy Steel
Bohler-Uddeholm BÖHLER M268 VMR® Plastic Mold Steel
Arkema Rilsamid® AMN BLACK P20 TLD PA12
AISI Type P20 Mold Steel (UNS T51620)

NCHIN024 / 78866

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.