MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

HB Fuller 22TL Threadlocking Adhesive and Sealant
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: 22TL is a thixotropic anaerobic compounds formulated to cure rapidly and reliably on most “as received” fasteners. They give predictable lubricity on assembly.

Features and Benefits:

  • 100% Solids
  • Bolt Threading Range from #2 to 1/2 inch (2.2 to 12 mm)
  • MIL (S-46163-A) Type II Grade M

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/cc
Brookfield Viscosity 1200 cP1200 cP
Storage Temperature 8.00 - 28.0 °C46.4 - 82.4 °F
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 4.10 MPa595 psiPin/Collar; ISO 10123
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 175 °C347 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Flash Point >= 93.0 °C>= 199 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 - 30.0 min0.167 - 0.500 hourHandling Strength
 360 - 4320 min6.00 - 72.0 hourFull cure
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorPurple
ConsistencyThixotropic Liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHBFULL142 / 316933

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.