MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ THERMOCOMP™ Compound WC006 Polybutylene Terephthalate (PBT) (Asia)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: LNP THERMOCOMP WC006 compound is based on Polybutylene Terephthalate (PBT) resin containing 30% carbon fiber. Added features of this grade include: Electrically Conductive.

Features: High Stiffness,Light-weight Structural,Super Strong (Carbon Fiber Filled),Electrically Conductive,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.43 g/cc0.0517 lb/in³ASTM D792
 1.43 g/cc0.0517 lb/in³ISO 1183
Moisture Absorption 0.0500 %0.0500 %Injection Molding
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/in24hrs; ASTM D955
 0.0023 cm/cm0.0023 in/in24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.012 cm/cm0.012 in/in24hrs; ISO 294
 0.010 - 0.020 cm/cm0.010 - 0.020 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 158 MPa22900 psiASTM D638
 158 MPa22900 psiISO 527
Tensile Strength, Yield 158 MPa22900 psiASTM D638
 158 MPa22900 psiISO 527
Elongation at Break 1.2 %1.2 %ASTM D638
 1.2 %1.2 %ISO 527
Elongation at Yield 1.2 %1.2 %ASTM D638
 1.2 %1.2 %ISO 527
Tensile Modulus 19.99 GPa2899 ksi50 mm/min; ASTM D638
 20.66 GPa2996 ksi1 mm/min; ISO 527
Flexural Strength 206 MPa29900 psiASTM D790
 219 MPa31800 psiISO 178
Flexural Modulus 15.16 GPa2199 ksiASTM D790
 17.0 GPa2470 ksiISO 178
Izod Impact Notched 42.0 J31.0 ft-lbASTM D256
Izod Impact, Unnotched 4.64 J/cm8.69 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 4.00 kJ/m²1.90 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 30.0 kJ/m²14.3 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 8.00 J5.90 ft-lbpeak; ASTM D3763
Impact Test 2.00 J1.48 ft-lbMultiaxial Impact; ISO 6603
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  12.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
6.67 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 12.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
7.00 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow  68.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
37.8 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 68.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
37.8 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 223 °C433 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 222 °C
@Thickness 3.20 mm
432 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 209 °C408 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 211 °C
@Thickness 3.20 mm
412 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 245 - 255 °C473 - 491 °F
Zone 3 260 - 270 °C500 - 518 °F
Melt Temperature 240 - 265 °C464 - 509 °FInjection Molding
Mold Temperature 80.0 - 100 °C176 - 212 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81950 / 289897

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.