MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Phillips 66 Tacna® Rx NLGI No. 1
Categories: Fluid; Lubricant; Lithium Gellant; Organic Soap Gellant

Material Notes: Description: Conoco Tacna Rx is a multipurpose, lithium-complex, polymer-enhanced grease designed for a wide range of applications, including passenger cars, agricultural equipment, race cars, motorcycles, on- and off-road trucks, buses, vans and construction equipment. It also is suited for industrial applications such as the heavily loaded antifriction and plain bearings found in gear boxes and electric motors commonly used in steel and aluminum manufacturing plants, as well as in mining equipment that requires a water-resistant, high-temperature grease. It is dyed red for easy identification and leak detection. Certified for use wherever NLGI GC-LB quality grease is recommended.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 93Viscosity Index (Base Oil Property)
Saybolt Viscosity at 100°F 795 SUSBase Oil Property
Saybolt Viscosity at 210°F 77 SUSBase Oil Property
Kinematic Viscosity at 40°C (104°F) 151 cStBase Oil
Kinematic Viscosity at 100°C (212°F) 14.4 cStBase Oil
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Load Wear Index 40
Four Ball Extreme Pressure, Weld Load 400 kg
Four Ball Wear 0.430 mm
Penetration P(60), 1/10 mm 320
Timken Test 55.0 lb
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -10.0 °F
Dropping Point 500 °F
 
Descriptive Properties
ASTM Rust Test (A & B)Pass
ColorRed
Oxidation Resistance3 psi drop/100 hrs
Soap Type (Thickener)Lithium Complex
Water Washout0.05100°F
 0.08175°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON237 / 75274

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.