MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Phillips 66 TCS Slideway Lubricant ISO Grade 220
Categories: Fluid; Lubricant

Material Notes: TCS Slideway Lubricant is a premium quality circulating oil developed for the lubrication of lathes and heavily loaded machine tool slideways. It is specially formulated to prevent stick-slip problems to ensure good surface finish on the machined part, and to provide quick and effective separation from water and metalworking fluids. TCS Slideway Lubricant is specially formulated to allow machine tool carriages to start easily and move smoothly throughout their travel, thus preventing stick-slip problems. This reduces carriage chatter and ensures a smooth finish on the machined part. Mild extreme-pressure properties prevent scoring of the slideways during carriage travel. A tackiness additive improves adhesion and prevents the oil from being squeezed off the slideways. It also helps prevent the oil from being washed away by cutting fluids. Additional proprietary additives provide protection against rust and corrosion and allow optimum separation from coolants and tramp oils. TCS Slideway Lubricant is water-white in color to allow easy visibility of machined parts.

Applications:

  • Horizontal and vertical slideways on machine tools, such as lathes, planers, shapers, drilling machines, milling machines and screw machines
  • Printing presses
  • Lumber mill saw carriages
  • Other applications that require a clear, tacky slideway oil
Features/Benefits:
  • Excellent anti-stick-slip performance
  • Excellent coolant-separating properties
  • Good surface finish
  • Protects against scoring and wear
  • Good adhesion for retention on slideways
  • Protects against rust and corrosion
  • Water-white in color for easy visibility

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.874 g/cc0.874 g/cc
Density 0.872 g/cc0.0315 lb/in³
Viscosity Measurement 131131Index
Saybolt Viscosity at 100°F 1184 SUS1184 SUS
Saybolt Viscosity at 210°F 118 SUS118 SUS
Kinematic Viscosity at 40°C (104°F) 227 cSt227 cSt
Kinematic Viscosity at 100°C (212°F) 23.8 cSt23.8 cSt
ASTM Color 0.000.00ASTM D1500
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 1.31.3[mg KOH/g]; ASTM D974
 
Thermal PropertiesMetricEnglishComments
Pour Point -12.0 °C10.4 °F
Flash Point 280 °C536 °FCOC
 
Descriptive Properties
Demulsibility20 minutes to passASTM D1401
Slip<0.8Stick-Slip, ASTM D2877

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON5241 / 198494

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.