MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik VESTAMID® L-GF30 BK 9.7503 Nylon 12, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 30% Glass Fiber Filled

Material Notes: VESTAMID® L-GF30 BK 9.7503 is a glass fiber–reinforced heat stabilized Polyamide 12 for injection molding. The material contains about 30% glass fibers, an ageing protective agent and a processing aid for a fast and even form filling. Due to the reinforcement moldings from this compound exhibit a higher strength and good heat resistance. Further advantages of VESTAMID® L-GF30 BK 9.7506 are the characterizing properties of PA12, e.g., low water absorption, good dimensional stability and nearly constant mechanical properties at changing ambient humidity. VESTAMID® L-GF30 BK 9.7503 is supplied as cylindrical granules, ready for processing, in moisture-proof bags. Pigmentation may affect values. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
Dry properties listed below
Industrial Sector: Sustainable, Industry and Engineering
Sustainability: Sustainable electricity
Processing: Injection molding
Delivery form: Pellets, Granules
Optics: Laser absorbing
Resistance to: Heat (thermal stability)
Additives: Glass fibers
Applications: Encapsulation
Special Characteristics: High heat resistant
Color: Black
Additives: Antioxidant agent, Heat stabilizer, Processing aids

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 120 MPa17400 psiISO 527
Tensile Strength 121 MPa17500 psiISO 527
Tensile Strength, Yield 121 MPa17500 psiISO 527
Elongation at Break 6.00 %6.00 %Nominal; ISO 527
Elongation at Yield 5.00 %5.00 %ISO 527
Tensile Modulus 7.10 GPa1030 ksiISO 527
Charpy Impact Unnotched  9.00 J/cm²
@Temperature 23.0 °C
42.8 ft-lb/in²
@Temperature 73.4 °F
Type of failure: C; ISO 179/1eU
 10.0 J/cm²
@Temperature -30.0 °C
47.6 ft-lb/in²
@Temperature -22.0 °F
Type of failure: C; ISO 179/1eU
Charpy Impact, Notched  2.10 J/cm²
@Temperature -30.0 °C
9.99 ft-lb/in²
@Temperature -22.0 °F
Type of failure: C; ISO 179/1eA
 2.30 J/cm²
@Temperature 23.0 °C
10.9 ft-lb/in²
@Temperature 73.4 °F
Type of failure: C; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 178 °C352 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 175 °C347 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 165 °C329 °FISO 75-1/-2
Vicat Softening Point  175 °C
@Load 1.02 kg
347 °F
@Load 2.25 lb
50 K/h; ISO 306
 175 °C
@Load 5.10 kg
347 °F
@Load 11.2 lb
50 K/h; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 °C482 °FInjection Molding; ISO 294
Mold Temperature 80.0 °C176 °FInjection Molding; ISO 294
Injection Velocity 200 mm/sec7.87 in/secInjection Molding; ISO 294
 
Descriptive Properties
Blue water consumption23.9 kgISO 14040, 14044
ColorBlack
Global Warming Potential2.4 kg CO2 eq./kgsavings incl. bio. C. as compared to classical production, ISO 14040, 14044
 4.9 kg CO2 eq./kgincl. bio. C incl. LUC, ISO 14040, 14044
 4.9 kg CO2 eq./kgexcl. bio. C incl. LUC, ISO 14040, 14044
Land use (ReCiPe 2016)0.3 Annual crop eq. yISO 14040, 14044

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7916 / 325048

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.