MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Cushion-Mount™ E1840H Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion
Categories: Polymer; Adhesive

Material Notes: 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for combination printing, process printing, solids and line work. 3M now offers a range of 40 and 60 mil cushioned plate mounting tapes for flexographic printing needs.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.560 g/cc0.0202 lb/in³
Thickness 114 microns4.50 milFilm Liner
 1070 microns42.0 milTape
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 0.138 MPa20.0 psi10% Compression, Deflection
 0.276 MPa40.0 psi25% Compression, Deflection
Peel Strength 0.38347 kN/m2.1875 pliLinered side-Photopolymer, Adhesion; ASTM D3330
 0.60259 kN/m3.4375 pliNon-linered side-Composite Sleeve, Adhesion; ASTM D3330
 0.60259 kN/m3.4375 pliNon-linered side-Polyester, Adhesion; ASTM D3330
 0.60259 kN/m3.4375 pliNon-linered side-Urethane-B, Adhesion; ASTM D3330
 0.657 kN/m3.75 pliNon-linered side-Stainless Steel, Adhesion; ASTM D3330
 0.71216 kN/m4.0625 pliNon-linered side-Urethane-A, Adhesion; ASTM D3330
 
Descriptive Properties
LinerFirm Blue Foam

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM33948 / 168695

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.