MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
AISI 9255 Steel, normalized at 900°C (1650°F), 13 mm (0.5 in.) round
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 9000 Series Steel; Low Alloy Steel; Carbon Steel; Medium Carbon Steel

Key Words: AFNOR 55 S 7, UNI 55 Si 8, SS14 2085 (Sweden), B.S. 250 A 53, UNS G92550, ASTM A322, ASTM A519, SAE J404, SAE J412, SAE J770, DIN 1.0904
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 277
Hardness, Knoop 302Converted from Brinell
Hardness, Rockwell B 99Converted from Brinell
Hardness, Rockwell C 28Converted from Brinell hardness value.
Hardness, Vickers 292Converted from Brinell hardness value.
Tensile Strength, Ultimate 951 MPa
Tensile Strength, Yield 585 MPa
Elongation at Break 20 %in 50 mm
Modulus of Elasticity 200 GPaTypical for steel
Bulk Modulus 160 GPaTypical for steel
Poissons Ratio 0.29Calculated
Machinability 40 %hot rolled and cold drawn. Based on 100% machinability for AISI 1212 steel.
Shear Modulus 80.0 GPaTypical for steel
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000174 ohm-cmEstimated
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.5 µm/m-°C
@Temperature 20.0 °C
Estimated
 12.2 µm/m-°C
@Temperature 250 °C
Estimated
 13.9 µm/m-°C
@Temperature 500 °C
Estimated
 14.7 µm/m-°C
@Temperature 1000 °C
Estimated
Specific Heat Capacity 0.472 J/g-°CEstimated
Thermal Conductivity 51.9 W/m-KTypical steel
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.51 - 0.59 %
Iron, Fe 96.185 - 96.99 %As remainder
Manganese, Mn 0.70 - 0.95 %
Phosphorus, P <= 0.035 %
Silicon, Si 1.8 - 2.2 %
Sulfur, S <= 0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 9255 Steel, oil quenched from 885°C (1625°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
AISI 9255 Steel, oil quenched from 885°C (1625°F), 595°C (1100°F) temper, 13 mm (0.5 in.) round
AISI 9255 Steel, normalized at 900°C (1650°F)
AISI 9255 Steel, oil quenched from 885°C (1625°F), 650°C (1200°F) temper, 13 mm (0.5 in.) round
AISI 9255 Steel, normalized at 900°C (1650°F), 25 mm (1 in.) round

M925AD / 8631

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.