MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Vitro Minerals CS 200 Recycled Glass Powder
Categories: Ceramic; Glass

Material Notes: CS Glass powders are functional glass fillers and extenders made from 100% recycled glass. The products are white to off-white colored powders with a uniform particle size distribution. X-ray diffraction and scanning electron microscopy confirm that the CS Glass powders are fully amorphous and contain no crystalline silica. CS Glass powders provide a clean post consumer filler for polymer-based systems where the highest brightness is not required. The fillers impart excellent abrasion resistance and chemical stability to coatings and other polymer systems. Vitro Minerals’ unique processing system and true particle size classification provides consistent product quality for three grades with finenesses covering a range of potential applications: CS-200 (d50 = 12-16 µm); CS-325 (d50 = 10-12 µm); and CS-400 (d50 = 6-8 µm).

Information provided by Vitro Minerals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.50 g/cc2.50 g/ccASTM D1530
Bulk Density 1.01 g/cc0.0365 lb/in³ASTM C110
Brightness 78 - 83 %78 - 83 %
Fineness 2.02.0Hegman; ASMT D1210
Moisture Absorption at Equilibrium <= 0.50 %<= 0.50 %Free; ASMT C566
Particle Size 12 - 16 µm12 - 16 µmd50 median; Laser interferometer
 100 µm100 µmd98 top; Laser interferometer
Particle Mesh Size 325 Mesh325 Mesh80-90%; ASTM C25
pH 10 - 1110 - 11AFS 113-87-S
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 5.55.5
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.561.56ASTM D801
 
Component Elements PropertiesMetricEnglishComments
Al2O3 1.0 - 10 %1.0 - 10 %
B2O3 0.00 - 5.0 %0.00 - 5.0 %
CaO 5.0 - 15 %5.0 - 15 %
Fe2O3 <= 1.0 %<= 1.0 %
K2O <= 1.0 %<= 1.0 %
Loss on Ignition(%) <= 1.0 %<= 1.0 %
MgO <= 1.5 %<= 1.5 %
Na2O 1.0 - 15 %1.0 - 15 %
SiO2 50 - 80 %50 - 80 %
TiO2 <= 0.10 %<= 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CVITRO904 / 209578

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.