Varcum 29324 is a two-step, powdered phenolic resin. APPLICATION: A modifier for slow-curing resins used in the production of grinding wheels. FEATURES: Provides quicker setting of the resin bond, thereby reducing wheel processing difficulties related to soft bond structure in the early stages of oven baking. Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp) |