ATOFINA Polypropylene PPC 3645 is a nucleated heterophasic copolymer. PPC 3645 is characterized by improved stiffness, creep resistance and high impact resistance. Application PPC 3645 has been developed specifically for the extrusion of corrugated cardboard, corrugated and twin walled pipes, conduit pipe and other extrusion applications.Information provided provided by Total Petrochemicals. Total Petrochemicals acquired former Fina and Atofina plastics product lines. |