MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Avient Catize® WBP-3 Inherently Conductive Polymer/metal mixtures  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic

Material Notes:

Description/Features:

  • A mixture of an Inherently Conductive Polymer and metal particles.

Applications:

  • Coil coating
  • Industrial maintenance coatings
  • Marine Coatings
  • OEM coatings
  • Rebar & Bridge Coatings
  • Fastener Coatings

Processing Method:

  • Can be processed with normal dispersing equipment, such as high speed dispersers
  • for optimal results, contact PolyOne's technical staff to determine recommended processing.

Catize WBP-3 has been tested in several finished coating formulations as a post-add additive. It performs better on non-pretreated surfaces. Adequate cure time should be allowed prior to accelerated corrosion testing. Topcoating is not required for excellent salt spray results.

Disclaimer: Catize corrosion control additives are made under license of GeoTech's U.S. Pat. Nos. 5,976,419; 6,231,789; 6,440,332; 6,627,117 and other patents pending.

Information provided by PolyOne Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 20 - 25 %20 - 25 %
Particle Size 15 - 25 µm15 - 25 µmParticle size of the metal
 
Descriptive Properties
ColorBlue/Grey
Inherently Conductive Polymer TypePoly(3,4 ethylenedioxythiophene) PEDT/PSSA
Metal Particle typeAluminum
Product FormLiquid
Solvent TypeWater

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyram Metal Cap PPC373B72 Polypropylene, 72% mineral Filled
Polyram Metal Cap PPC372B73 Polypropylene, 73% Mineral Filled
Ecomass® 1850ZG92 Metal Filled Polyamide
Ecomass® 1850ZG90 Metal Filled Polyamide
Ecomass® 1080ZG90 Metal Filled Polyamide

PH1PO0016 / 43331

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.