MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Gougeon Brothers West System® 105 Epoxy Resin® / 207 Special Clear Hardener™
Categories: Polymer; Thermoset; Epoxy

Material Notes: 105/207 Epoxy is used for coating and fiberglass cloth application where an exceptionally clear, moisture-resistant, natural wood finish is desired. 105/207 is blush free and will not turn cloudy in humid conditions. Thin film applications roll out and tip off smoothly, requiring less sanding in preparation for finish coatings. Three coats or more can be applied in one day without additional surface preparation. Fewer coats are required to fill fiberglass weave and in most cases the final coating can be sanded the following day. 105/207 forms a high-strength, moisture-resistant solid with excellent bonding and barrier coating properties and is used as a structural adhesive for gluing and laminating. It has excellent compatibility with paints and varnishes. An ultraviolet inhibitor in 207 helps provide a beautiful, long lasting finish when used with quality UV-filtering varnish. It is formulated without volatile solvents resulting in a very low VOC content. It has a relatively high flash point, no strong solvent odor and does not shrink after curing.

Information provided by Gougeon Brothers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/cc
Viscosity 760 cP760 cPMixed; ASTM D-2393
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 84.484.4ASTM D-2240
Tensile Strength 46.5 MPa6750 psiASTM D638
Elongation at Break 3.8 %3.8 %ASTM D638
Tensile Modulus 3.03 GPa440 ksiASTM D638
Flexural Strength 77.9 MPa11300 psiASTM D-790
Flexural Modulus 2.84 GPa412 ksiASTM D-790
Compressive Yield Strength 75.8 MPa11000 psiASTM D-695
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 47.2 °C117 °FASTM D-648
Glass Transition Temp, Tg 46.7 °C116 °FOnset
 46.7 °C116 °FUltimate
 
Processing PropertiesMetricEnglishComments
Cure Time 600 - 900 min10.0 - 15.0 hoursolid, thin film
 1440 - 5760 min24.0 - 96.0 hourworking strength
Pot Life 22.0 - 26.0 min22.0 - 26.0 min100 g
Working Life 110 - 120 min110 - 120 minThin film
 
Descriptive Properties
Mix ratio3 parts resin: 1 part hardenervolume, 300 Mini Pump ratio
 3.64 : 1weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOUGW904 / 290748

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.