MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Synthos WELLITE™ AS-90 Phenolic Resin for Abrasive
Categories: Polymer; Thermoset; Phenolic

Material Notes: This series of phenolic resins are applied to bonded abrasives and are available in powder and liquid form. Due to strict formula design, effective molecular weight and distributing control method, the distribution of resin molecular reaches an ideally narrow status
  • The powder resin is characterized in strong viscosity, mechanical strength, abrasion resistance, heat resistance and wet grinding stability.
  • The liquid resin has good wetting function, anti-moisture properties and well-distributed miscibility, and maintain high strength and grinding performance.
Application: General ultra-thin disc

Information provided by Sundow Polymers Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesOriginal ValueComments
Cure Time 90.0 - 120 sec
@Temperature 150 °C
 
Descriptive Properties
AppearanceLight yellow powder
Content<1.5%Free phenol
Granularity99% under200 mesh
Inclined plate flow40-60 mm125°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSUNDOW072 / 320103

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.