MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Altron™ PPO Polyphenylene oxide, unfilled, extruded (ASTM Product Data Sheet)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO

Material Notes:

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccASTM D792
Water Absorption 0.10 %Immersion, 24hr; ASTM D570(2)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 92ASTM D785
Tensile Strength 8300 psiASTM D638
Tensile Strength at 65°C (150°F) 4000 psiASTM D638
Elongation at Break 23 %ASTM D638
Tensile Modulus 367 ksiASTM D638
Flexural Strength 12900 psiASTM D790
Flexural Modulus 397 ksiASTM D790
Compressive Strength 13200 psi10% Def.; ASTM D695
Compressive Modulus 316000 psiASTM D695
Shear Strength 8300 psiASTM D732
Izod Impact, Notched 2.90 ft-lb/inASTM D256 Type A
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square >= 1e+13 ohmEOS/ESD S11.11
Dielectric Strength 701 V/milShort Term; ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 35.6 µin/in-°F
@Temperature -40.0 - 149 °C
ASTM E831
Maximum Service Temperature, Air 200 °FLong Term
Deflection Temperature at 1.8 MPa (264 psi) 260 °FASTM D648
Glass Transition Temp, Tg 284 °FASTM D3418
Flammability, UL94 V-1
@Thickness 3.17 mm
Estimated Rating
 
Compliance PropertiesOriginal ValueComments
3A-Dairy No
Canada AG No
FDA No
USDA No
USP Class VI No
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Unacceptable
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Unacceptable
Conductive / Static Dissipative No
Continuous Sunlight Limited
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Limited
Hydrocarbons - Aromatic Unacceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Unacceptable
 
Descriptive Properties
ColorBlack
Machinability61-10, 1=Easier to Machine

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ensinger NORYL® Polyphenylene oxide (PPO)
Overview of materials for PPE/PPO + Carbon Fiber
BASF Ultramid® 1503-2 NF2004 33% Glass Filled PA66 (Conditioned)
Mitsubishi Chemical Advanced Materials Ketron® 1000 PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Data Sheet)
EPICHEM Epiryl PPO V0 Polyphenylene oxide

P1SM10A / 20085

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.