Product Description: HTA 001HP2 is a high molecular weight HDPE film grade providing very good processability on high output extruders. Films made from HTA 011HP2 exhibit excellent impact and toughness properties as well as high stiffness. Availability: Africa & Middle East, Asia Pacific and Europe Additive: - Antiblock: No
- Slip: No
- Thermal Stabilizer: Yes
Applications: - Blown Film
- Grocery Sacks
- Liners
- Refuse Bags
- Shoppers
- Thin Gauged Consumer Bags
Information provided by ExxonMobil |