Hostacom TRC 2157N C NATURAL is a 18% talc filled PP copolymer, with high flowability, good impact/stiffness balance, high UV resistance, very good scratch resistance and low emissions. This grade is not intended for medical, pharmaceutical, food and drinking water applications. Availability: Asia-Pacific Application: Automotive Parts; Interior Trims Market: Automotive Attribute: Good Moldability Information provided by LyondellBasell. |