KEBAFLOW LCP MF235 is a high heat resistance LCP reinforced with 35% short glass fibers. The material is characterized by the following properties: Good flowability at thin wall thicknesses, very good toughness and strength, inherent flame retardancy, high heat deflection temperature (HDT /A = 255°C), good chemical resistance. Compared to other LCP grades, KEBAFLOW MF235 exhibits significantly improved weld line strength. Properties: dimensionally stable, Thin wall thicknesses, good aging behavior, good fire behavior, high continuous used temperature, semi-crystalline, high continuous used temperature Information provided by BARLOG plastics GmbH. |