MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Invista T 94 PET Copolymer Packaging Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Acetaldehyde content: <2 ppm.
Fines 0.1% through 28 mesh as manufactured.
Moisture content <0.3% as manufactured.
Chip size 85±15 pellets/g.
Crystallinity >50%.

T 94 PET is a copolymer packaging resin with a nominal intrinsic viscosity of 0.84 dl/g engineered for big plastic jug applications. It has excellent melt and crystallization properties, offering easy processibility in injection molding and stretch-blow molding.

Packaging made from this resin has excellent clarity and is noted for its crystallization rate, which imparts an excellent clarity and gloss to the container. It conforms to FDA regulation. Widely used in applications such as 5 gallon jugs, food containers, and other custom containers.

Information supplied by the manufacturer.

The Invista PET product line has been acquired by Indorama.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.840 g/cc0.0303 lb/in³M2E-72-015 test
Density 1.389 - 1.399 g/cc0.05018 - 0.05054 lb/in³M2E-71-065 test
Viscosity Measurement 0.82 - 0.860.82 - 0.86Intrinsic viscosity; WI No. 104 test; correlated from solution viscosity by Invista
 
Thermal PropertiesMetricEnglishComments
Melting Point >= 238 °C>= 460 °FM2E-72-047 test

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sibur TVERPET® Polyethylene Terephthalate (PET)
SK Chemicals SKYPET® BL8450 Specially Formulated PET Copolymer Resin
Eastman 9921 PET Injection Molded
DAK Americas Laser+® HP806 (B93A) PET
DAK Americas Laser+® C91A PET

PKO250 / 48905

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.