MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Geon® Performance Solutions Vinyl Rigid Extrusion 6922  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.45 g/cc1.45 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 83
@Time 15.0 sec
83
@Time 0.00417 hour
ASTM D2240
Tensile Strength, Yield 46.3 MPa6720 psiType I, 5.1 mm/min; ASTM D638
Tensile Modulus 3.09 GPa448 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 83.8 MPa12200 psiASTM D790
Flexural Modulus 3.03 GPa439 ksiASTM D790
Izod Impact, Notched  0.801 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
1.50 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Across Flow, Compression Molded; ASTM D256A
 0.961 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
1.80 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Flow, Compression Molded; ASTM D256A
 11.0 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Dart Drop Total Energy  61.8 J/cm
@Temperature 23.0 °C
0.116 ft-lb/mil
@Temperature 73.4 °F
Procedure A, C.125 Dart; ASTM D4226
 178 J/cm
@Temperature 23.0 °C
0.333 ft-lb/mil
@Temperature 73.4 °F
Procedure B, C.125 Dart; ASTM D4226
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 61.0 µm/m-°C33.9 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 71.7 °C
@Thickness 3.18 mm
161 °F
@Thickness 0.125 in
Unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 193 °C360 - 379 °F
 
Descriptive Properties
FormsPellets
PVC Cell Classification1-41444-33ASTM D4216
 16364ASTM D1784
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PH1PN8731 / 102567

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.