MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Phillips 66 76® Lubricants Firebird LD Motor Oil SAE Grade 5W-20  (discontinued **)
Categories: Fluid; Lubricant

Material Notes: 76® Firebird LD Motor Oil is an environmentally responsible, part-synthetic automotive engine oil designed to provide excellent engine protection for gasoline-fueled and flex-fuel passenger cars and light trucks under all operating conditions. It is formulated with a blend of synthetic and high-quality re-refined base stocks. The use of re-refined base stocks helps lessen the environmental impact of disposal of used oil. Firebird LD Motor Oil is formulated to provide excellent wear protection, to minimize sludge and varnish formation, and to resist viscosity and thermal breakdown, even in severe service. It also protects against rust and bearing corrosion, and is resistant to foaming. The part-synthetic formulation provides enhanced performance benefits at extreme temperatures compared with conventional engine oils, for extra protection under all driving conditions. Firebird LD Motor Oil is fully licensed by the API and meets new car warranty requirements as defined by ILSAC GF-5. It meets “Resource Conserving” requirements for fuel economy improvement, emission system and turbocharger protection, and protection of engines operating on ethanol-containing fuels up to E85. It is backward serviceable for use where API SM or earlier “S” category engine oils are recommended.

Applications:

  • Gasoline-fueled and flex-fuel passenger cars, light trucks and sport utility vehicles
Firebird LD Motor Oil is licensed for:
  • ILSAC GF-5
  • API Service SN with Resource Conserving
Firebird LD Motor Oil meets or exceeds the requirements of:
  • Chrysler MS-6395 (Rev. T)
  • Ford WSS-M2C945-A (SAE 5W-20), WSS-M2C946-A (SAE 5W-30)
  • GM6094M (obsolete)
Features/Benefits:
  • Meets ILSAC GF-5 requirements for new cars under warranty
  • Friction-modified for improved fuel economy
  • Resists viscosity and thermal breakdown at high temperatures
  • Protects against sludge and varnish formation
  • Protects against wear
  • Protects against rust and bearing corrosion
  • Good low-temperature pumpability for easier cold starts
  • Good foam resistance
  • Formulated to protect turbochargers and emissions control system catalysts
  • Formulated for use in vehicles operating on ethanol-containing fuels up to E85
  • Lessens the environmental impact of disposal of used oil

Information provided by Phillips 66 Lubricants. The 76® Lubricants brand name was consolidated into other Phillips 66 brands in 2016; many products remain available under a new name.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.866 g/cc
Density 7.21 lb/gal
Viscosity 3.1 cP
@Temperature -150 °C
High-Temp/High-Shear
 5600 cP
@Temperature -30.0 °C
Cold Cranking
Viscosity Measurement 159Index
Kinematic Viscosity at 40°C (104°F) 49 cSt
Kinematic Viscosity at 100°C (212°F) 8.5 cSt
Ash 0.96 %Sulfated; ASTM D874
ASTM Color 3.5ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Base Number 8.0ASTM D2896
 
Thermal PropertiesOriginal ValueComments
Pour Point -39.0 °C
Flash Point 220 °CCOC
 
Component Elements PropertiesOriginal ValueComments
Phosphorus, P 0.077 %
Zinc, Zn 0.085 %
 
Descriptive Properties
Composition>50%Re-refined Content, Finished Oil

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON6390 / 210080

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.