Treatment required for max strength: as supplied Formability Ratio, 90° Bend, Radius/Thickness (Good Way): 0.5 Formability Ratio (bad Way): 0.5 Superficial Hardness: 30T 69-75Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman. Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011. |