MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Ganpati Exim No. 60 Fully Refined Paraffin Wax
Categories: Other Engineering Material

Material Notes: Paraffin is a common name for a group of alkane hydrocarbons. It is distinct from the fuel known in Britain as paraffin oil or just paraffin. The solid forms of paraffin are called paraffin wax. Paraffin is also a technical name for an alkane in general, but in most cases it refers specifically to a linear or normal alkane, while branched, or isoalkane are also called isoparaffins.

Uses: Candle & decorative candle/Wax wr5apping paper/Raw material for shoe polish, polish, etc. /for batik producers/to make matches.

Information provided by Ganpati Exim PVT. LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Penetration <= 18Needle, GB/T4985
 
Thermal PropertiesOriginal ValueComments
Melting Point 60.0 - 62.0 °CGB/T2539
 
Descriptive Properties
Color>25GB/T3554
Content<0.5%Oil, GB/T3554
Light Stability<5GB/T0404

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGANPATI087 / 317371

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.