MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Reynolds Smooth-Cast® 61D Semi-Rigid Urethane Casting Resins
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Product Overview: The Smooth-Cast™ Semi-Rigid line of low-cost semi-rigid urethane casting resins cure quickly to semi-rigid plastics that offer exceptional strength and impact resistance. New Formulations – New Look! Smooth-Cast 45D, 60D and 61D are newly reformulated with a translucent white appearance and improved physical properties. All Smooth-Cast semi-rigids are now mercury free and phthalate free. These plastics are easy-to-use (mix ratio is 1A:1B by volume) and have low viscosities for minimal bubble entrapment. Vibrant colors are possible by adding SO-Strong™, UVO™ or Ignite™ colorants.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccASTM D-1475
Viscosity 430 cP430 cPMixed; ASTM D-2393
Linear Mold Shrinkage 0.0125 cm/cm0.0125 in/inASTM D-2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6161ASTM D-2240
Tensile Strength, Ultimate 16.7 MPa2420 psiASTM D-638
Elongation at Break 100 %100 %ASTM D-638
Tensile Modulus 0.113 GPa16.4 ksiASTM D-638
Flexural Strength 2.41 MPa350 psiASTM D-790
Flexural Modulus 0.0607 GPa8.80 ksiASTM D-790
Compressive Strength 6.55 MPa950 psiASTM D-695
Compressive Modulus 0.0283 GPa4.10 ksiASTM D-695
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min1.00 hourHandling Time
Pot Life 7.00 min7.00 minASTM D-2471
 
Descriptive Properties
ColorTranslucent White
Mix Ratio100A:93Bby weight
 1A:1Bby volume
Specific Volume26.4[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN012 / 296713

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.