Description: HexPly® XF3+V24 is a new range of epoxy surface film providing excellent surface finish and requiring minimum preparation for painting. It is suitable for automotive parts that require an excellent surface finish. HexPly® XF3+V24 is co-curable with a range of HexPly® prepregs that can cure at 120°C and 180°C. It is available in 300 gsm. Features: - Easy to handle, good tack and drapability.
- Easy to sand.
- Can be co-cured with HexPly® M10R, M49, M47.
- Excellent resistance to aging tests (eg: +80/-40°C cycles up to 80% relative humidity).
Information provided by Hexcel Corporation. |