MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 7% Plasticizer  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Cellulosic; Cellulose Acetate Butyrate, Molded

Material Notes: Amorphous Cellulose Acetate Butyrate (CAB)

Characteristics: Dimensional Stability, Weatherability and Low Temp Impact Strength

Applications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and Toys

Processing: Injection Molding (Melt Temperature: 460°F, Mold Temperature: 150°F)

Data supplied by Albis Plastics Corporation.

Former ALBIS Plastics product lines have been spun off under the MOCOM brand. This specific grade was discontinued prior to the spin off.

Key Words: CAB
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Water Absorption 1.5 %1.5 %(24 hr); ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm0.0020 - 0.0060 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 40.0 MPa5800 psiASTM D638
Tensile Strength, Yield 34.5 MPa5000 psiASTM D638
Flexural Yield Strength 41.4 MPa6000 psiASTM D790
Flexural Modulus 1.31 GPa190 ksiASTM D790
Izod Impact, Notched 1.98 J/cm3.71 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FASTM D648
Vicat Softening Point 111 °C232 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 238 °C460 °FInjection
Mold Temperature 66.0 °C151 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo Plexiglas® V825-UVA5A Acrylic
Trinseo Plexiglas® V825 Acrylic
RTP Company PermaStat® 300 FR A Polycarbonate (PC), ESD Protection - Permanently Anti-static - Flame Retardant
RTP Company ESD 300 EM FR Polycarbonate (PC), ESD Protection - Static Dissipative - Flame Retardant - Easy Molding - UL94
Röhm Plexiglas® df21 8N Molding Compound

PZA1C23 / 21818

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.