MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ATSP Innovations NOWE™ 1130MCF Copolyester, 30% Milled Carbon Fibers
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: KEY CHARACTERISTICS:
  • Great wear properties and high toughness
  • Excellent weathering resistance
  • Excellent oxidative stability
  • High glass transition and heat deflection temperature
  • Non-flammable
  • Cryogenic-safe
  • Very low moisture pickup and high moisture resistance
  • Easy machinability – low dust
  • Radiation resistant
APPLICATIONS:
  • Sliding and linear contact bearings
  • Valves seats, pump components
  • Cages for roller bearings
  • Bushings
  • Thrust washers
  • Aerospace parts
  • Seals
  • Pad bearings

    This data was provided by ATSP Innovations

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 245 MPa35500 psiASTM D695
 340 MPa49300 psiISO 604
Compressive Modulus 8.50 GPa1230 ksiASTM D695
Coefficient of Friction 0.10 - 0.300.10 - 0.30typical dry; Maximum sliding speed 2.4 m/s
Limiting Pressure Velocity  1.00 MPa-m/sec
@Temperature 300 °C
28600 psi-ft/min
@Temperature 572 °F
 24.0 MPa-m/sec
@Temperature 25.0 °C
685000 psi-ft/min
@Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.0 µm/m-°C16.7 µin/in-°F
Maximum Service Temperature, Air 370 °C698 °F
Maximum Service Temperature, Inert 425 °C797 °F
Glass Transition Temp, Tg 230 °C446 °F
Flammability, UL94 V-0V-0
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) 0.10 %
@Temperature 311 °C
0.10 %
@Temperature 592 °F
Inert
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PESTHR02 / 243005

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.