MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil HD 6307 Blow Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Product Description: AExxonMobil™ HD 6307 is a medium molecular weight distribution high density polyethylene homopolymer. It possesses excellent processing uniformity and produces bottles with excellent appearance and rigidity. ExxonMobil™ HD 6307 offers the maximum in barrier properties available in high density polyethylene, and imparts minimum odor and taste to the packaged product.

Availability: Africa & Middle East, Latin America, North America and South America

Additive:

  • Thermal Stabilizer: Yes
  • Antistatic: No
Applications:
  • Food packaging
  • Liquid Food Containers for Milk, Water and Juices
  • Thermoformed Parts
Information provided by ExxonMobil Chemical

Key Words: Paxon™ AD60-007
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.963 g/ccASTM D4883
ESCR 100% Igepal® 8.0 hourASTM D1693 Condition B
Melt Flow 0.73 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 64.0
@Time 15.0 sec
ASTM D2240
Tensile Strength at Break 15.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 4700 psiASTM D638
Elongation at Yield 8.00 %ASTM D638
Flexural Modulus 160000 psi2% Secant; ASTM D790
Flexural Modulus, 1% Secant 190000 psi1.3 MM/MIN; ASTM D790
Charpy Impact, Notched 0.700 J/cm²
@Temperature -20.0 °C
ISO 179/1eA
 1.00 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 260 °FASTM D1525
 
Processing PropertiesOriginal ValueComments
Melt Temperature 273 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil HPA 020 Molding High Density Polyethylene (HMW) Resin
Oxford Polymers PC 1518 Unfilled Polycarbonate for Injection Molding
SCG Chemicals EL-Lene™ H5840B High Density Polyethylene Blow Molding
SCG Chemicals EL-Lene™ H6240B High Density Polyethylene Blow Molding
ExxonMobil HD 5705 High Density Polyethylene Resin

PEXB095 / 37400

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.