MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Overview of materials for Nylon 12, Extrusion/Tubing Grade
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Extrusion/Tubing Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.00 - 1.12 g/cc0.0361 - 0.0405 lb/in³Average value: 1.02 g/cc Grade Count:41
Water Absorption 0.0100 - 2.30 %0.0100 - 2.30 %Average value: 1.08 % Grade Count:4
Moisture Absorption at Equilibrium 0.500 - 0.700 %0.500 - 0.700 %Average value: 0.538 % Grade Count:13
Water Absorption at Saturation 1.00 - 1.50 %1.00 - 1.50 %Average value: 1.20 % Grade Count:6
Melt Flow 0.400 - 170 g/10 min0.400 - 170 g/10 minAverage value: 27.3 g/10 min Grade Count:24
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 61.0 - 73.061.0 - 73.0Average value: 66.7 Grade Count:15
Ball Indentation Hardness 64.0 - 76.0 MPa9280 - 11000 psiAverage value: 73.0 MPa Grade Count:4
Tensile Strength, Ultimate 28.0 - 44.0 MPa4060 - 6380 psiAverage value: 37.2 MPa Grade Count:5
Tensile Strength, Yield 20.0 - 76.0 MPa2900 - 11000 psiAverage value: 37.4 MPa Grade Count:41
Elongation at Break 50.0 - 400 %50.0 - 400 %Average value: 103 % Grade Count:49
Elongation at Yield 5.00 - 32.0 %5.00 - 32.0 %Average value: 17.1 % Grade Count:37
Modulus of Elasticity 0.332 - 2.23 GPa48.2 - 323 ksiAverage value: 0.912 GPa Grade Count:43
 0.259 - 0.441 GPa
@Temperature 40.0 - 100 °C
37.6 - 64.0 ksi
@Temperature 104 - 212 °F
Average value: 0.332 GPa Grade Count:1
Poissons Ratio 0.450 - 0.450
@Temperature 100 - 100 °C
0.450 - 0.450
@Temperature 212 - 212 °F
Average value: 0.450 Grade Count:1
Charpy Impact Unnotched 1000 J/cm² - NB4760 ft-lb/in² - NBGrade Count:35
 999.9 J/cm² - NB
@Temperature -40.0 - 0.000 °C
4759 ft-lb/in² - NB
@Temperature -40.0 - 32.0 °F
Grade Count:33
Charpy Impact, Notched 0.400 J/cm² - NB1.90 ft-lb/in² - NBAverage value: 3.80 J/cm² Grade Count:37
 0.100 - 9.40 J/cm²
@Temperature -40.0 - 0.000 °C
0.476 - 44.7 ft-lb/in²
@Temperature -40.0 - 32.0 °F
Average value: 0.921 J/cm² Grade Count:35
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+10 - 1.00e+15 ohm-cm1.00e+10 - 1.00e+15 ohm-cmAverage value: 9.88e+13 ohm-cm Grade Count:17
Surface Resistance 1.00e+12 - 1.00e+15 ohm1.00e+12 - 1.00e+15 ohmAverage value: 4.55e+14 ohm Grade Count:15
Dielectric Constant 3.00 - 15.03.00 - 15.0Average value: 6.13 Grade Count:14
Dielectric Strength 26.0 - 50.0 kV/mm660 - 1270 kV/inAverage value: 35.1 kV/mm Grade Count:17
Dissipation Factor 0.000304 - 0.3300.000304 - 0.330Average value: 0.120 Grade Count:14
Comparative Tracking Index 575 - 600 V575 - 600 VAverage value: 593 V Grade Count:13
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.0 - 252 µm/m-°C27.8 - 140 µin/in-°FAverage value: 110 µm/m-°C Grade Count:18
CTE, linear, Transverse to Flow 100 - 180 µm/m-°C55.6 - 100 µin/in-°FAverage value: 120 µm/m-°C Grade Count:8
Melting Point 171 - 180 °C340 - 356 °FAverage value: 176 °C Grade Count:29
Maximum Service Temperature, Air 75.0 - 150 °C167 - 302 °FAverage value: 113 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 90.0 - 140 °C194 - 284 °FAverage value: 109 °C Grade Count:15
Deflection Temperature at 1.8 MPa (264 psi) 40.0 - 165 °C104 - 329 °FAverage value: 56.7 °C Grade Count:18
Vicat Softening Point 115 - 175 °C239 - 347 °FAverage value: 143 °C Grade Count:19
Glass Transition Temp, Tg 13.0 - 130 °C55.4 - 266 °FAverage value: 67.8 °C Grade Count:4
Flammability, UL94 HB - V-2HB - V-2Grade Count:13
Oxygen Index 26.0 - 30.0 %26.0 - 30.0 %Average value: 27.3 % Grade Count:3
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 80.0 %80.0 %Average value: 80.0 % Grade Count:4
 
Processing PropertiesMetricEnglishComments
Processing Temperature 230 °C446 °FAverage value: 230 °C Grade Count:5
Die Temperature 230 °C446 °FAverage value: 230 °C Grade Count:5
Melt Temperature 190 - 280 °C374 - 536 °FAverage value: 224 °C Grade Count:10
Mold Temperature 40.0 - 60.0 °C104 - 140 °FAverage value: 50.0 °C Grade Count:10
Injection Velocity 100 mm/sec3.94 in/secAverage value: 100 mm/sec Grade Count:5
Die Opening 0.0400 cm0.0157 inAverage value: 0.0400 cm Grade Count:5
Roll Temperature 50.0 °C122 °FAverage value: 50.0 °C Grade Count:5
Drying Temperature 80.0 - 110 °C176 - 230 °FAverage value: 96.7 °C Grade Count:5
Injection Pressure 40.0 - 50.0 MPa5800 - 7250 psiAverage value: 45.0 MPa Grade Count:5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 12
Overview of materials for Nylon 6, Extruded
Overview of materials for Nylon 66, Extruded
Arkema Pebax® 5533 SA 01 MED Polyether Block Amide (PEBA)
Evonik Vestamid® Terra DD G16 Nylon 1012

O2645 / 78068

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.