MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ITW Insulation TRYMER® 6000 Polyisocyanurate Insulation
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: TRYMER™ 6000 insulation is a polyurethane modified polyisocyanurate cellular plastic. The rigid insulation is supplied in the form of bunstock for fabrication into sheets, pipe shells, tank and vessel coverings, and other shapes for a variety of thermal insulation applications. TRYMER™ 6000 insulation features improved dimensional stability over a wider range of temperatures than standard polyurethane insulation. TRYMER™ insulation is not a known nutrient source for mold and mildew.

Applications: TRYMER™ 6000 polyiso-cyanurate insulation is used extensively in industrial and commercial applications with high density/strength requirements, within the service temperature range of -297°F to +300°F (-183°C to +149°C). Typical applications for TRYMER™ 6000 insulation include:

  • industrial pipe insulation, including elbows and fittings pipe hangers, saddles and supports
  • tank and vessel insulation
  • core material for architectural and structural panels
  • core material for factory-built panelized constructions

Information provided by ITW Insulation Systems

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0960 g/ccASTM D1622
Water Absorption 0.70 %
@Time 86400 sec
immersion; ASTM C272
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 95.0 psiParallel to rise-thickness; ASTM D1623
Flexural Strength 160 psiparallel to rise; ASTM C203
Flexural Modulus 5800 psiparallel to rise; ASTM C203
Compressive Strength 130 psiPerpendicular to rise-width; ASTM D1621
 130 psiPerpendicular to rise-length; ASTM D1621
 140 psiParallel to rise-thickness; ASTM D1621
Compressive Modulus 2800 psiPerpendicular to rise-width; ASTM D1621
 2800 psiPerpendicular to rise-length; ASTM D1621
 3100 psiParallel to rise-thickness; ASTM D1621
Shear Modulus 800 ksiparallel to perpendicular, avg; ASTM C273
Shear Strength 80.0 psiparallel to perpendicular, avg; ASTM C273
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0290 W/m-KAged 180 days; ASTM C518
Maximum Service Temperature, Air 149 °C
Minimum Service Temperature, Air -183 °C
Flame Spread Index <= 25
@Thickness <=152 mm
ASTM E84
 
Descriptive Properties
Closed Cell Content95%ASTM D2845
ColorTan
Dimensional Stability+0.4% Changeat 70°C, 97% RH, 7 days, Length, ASTM D2126
 +0.5% Changeat 70°C, 7 days, Volume, ASTM D2126
 +0.7% Changeat 70°C, 97% RH, 7 days, Volume, ASTM D2126
 +1% Changeat 70°C, 7 days, Length, ASTM D2126
 -0.1% Changeat -40°C, 7 days, Volume, ASTM D2126
 -0.2% Changeat -23°C, 7 days, Length, ASTM D2126
 -0.3% Changeat -40°C, 7 days, Length, ASTM D2126
 -0.4% Changeat 149°C, 7 days, Length, ASTM D2126
 -0.7% Changeat -23°C, 7 days, Volume, ASTM D2126
 -1% Changeat 149°C, 7 days, Volume, ASTM D2126
R-Value0.93 (m²-°C)/Waged 180 days, ASTM C518
Surface Burning Characteristics450Smoke Developed, ASTM E84
Water Vapor Permeability1.1 perm-inchASTM E96

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWZ014 / 187080

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.