MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Eneos DYNARON®6201B/PP/oil 40/20/40 blend
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes:

ENEOS has acquired the elastomer product lines from JSR Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
30 g/10 min
@Load 4.77 lb,
Temperature 446 °F
JIS K7210
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6767JIS K6253
Tensile Strength 34.0 MPa4930 psi500mm/min; JIS K6251
Elongation at Break 550 %550 %500mm/min; JIS K6251
Compression Set  21 %
@Temperature 23.0 °C,
Time 79200 sec
21 %
@Temperature 73.4 °F,
Time 22.0 hour
JIS K6262
 64 %
@Temperature 70.0 °C,
Time 79200 sec
64 %
@Temperature 158 °F,
Time 22.0 hour
JIS K6262
 
Descriptive Properties
Oil Resistance0.0740°C, 72 hrs, JIS K6258, ASTM No.1
 0.4340°C, 72 hrs, JIS K6258, Fuel A
 0.5240°C, 72 hrs, JIS K6258, IRM903

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PJSRC8212 / 295528

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.