Trigonox B-C90 is an efficient initiator (90% active ingredient in odorless mineral spirits) for the production of Low-Density Polyethylene (LDPE). It is used for both tubular and autoclave processes. In most cases a combination with other peroxides is used to ensure a broad reactivity range. CAS number: 110-05-4 EINECS/ELINCS No: 203-733-6 Applications: Trigonox B-C90 is an efficient initiator for the production of Low-Density Polyethylene (LDPE). It is used both for tubular and autoclave processes. In most cases a combination with other peroxides is used to ensure a broad reactivity range. Information provided by Nouryon |