MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Thermal Ceramics K-shield BF Paper
Categories: Ceramic

Material Notes: K-Shield BF Paper is a totally organic-free paper produced from premium, cleaned Kaowool high-purity fibers in a unique paper-making process. The cleaning process of these special fibersimproves the thermal conductivity and insulating value of the product. K-Shield BF Paper offers excellent thermal resistance and good handling strength with no off-gassing.

Features:

  • 100% organic free with no outgassing
  • Low shot (unfiberized material) content
  • Very low thermal conductivity and heat storage
  • Excellent high-temperature parting agent
  • Thin, flexible high-temperature insulation
  • Good fired strength
  • Easily die-cut for gaskets
  • Applications:

  • Separating media to prevent sticking
  • Vacuum heat treating furnaces
  • Parting agent in brazing and heat treating
  • Powered Metal sintering
  • Applications that require good fired strengths
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 0.128 - 0.160 g/cc
     
    Mechanical PropertiesOriginal ValueComments
    Tensile Strength, Ultimate 15.0 - 25.0 psi
     15.0 - 25.0 psiFired
     
    Thermal PropertiesOriginal ValueComments
    Thermal Conductivity 0.380 BTU-in/hr-ft²-°F
    @Temperature 260 °C
     0.590 BTU-in/hr-ft²-°F
    @Temperature 538 °C
     0.850 BTU-in/hr-ft²-°F
    @Temperature 816 °C
     1.18 BTU-in/hr-ft²-°F
    @Temperature 1090 °C
    Melting Point 3200 °F
    Maximum Service Temperature, Air 2300 °F

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    CTHERM251 / 2571

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.