MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond Supreme 3DM-85 One component, toughened epoxy system
Categories: Polymer; Thermoset; Silicone

Material Notes: Key Features:
  • No mixing, convenient handling
  • Cures at 185°F
  • Reliable electrical insulator
  • Used as a barrier to block flow
Product Description: Master Bond Supreme 3DM-85 is a toughened, one part epoxy that can be used for bonding, sealing, and dam-and-fill applications. It is a no mix system with a curing schedule of 185°F for 2 to 3 hours. Aside from its use as an adhesive, it is also used for chip on board encapsulations. After curing, it blocks the flow of a second epoxy that is encapsulating chips and wire bonds. The curing temperature of 185°F is especially significant because it allows the epoxy to be used in applications where plastic substrates are sensitive to higher temperature curing profiles. This system is not premixed and frozen and its working life is unlimited at room temperature. Supreme 3DM-85 bonds well to a wide variety of substrates used in electronics including metals, composites, ceramics and many plastics. It has very good physical strength properties. The system is thermally conductive and electrically insulating. Also, it is a toughened system that can withstand various types of thermal cycling. The service temperature range is -100°F to +350°F. The color is black. While it is primarily used as a damming epoxy it can also be used for conventional bonding. Supreme 3DM-85 can be used for applications where a non-mixed epoxy is desirable and heat curing above 200°F is not possible.

Product Advantages:

  • One part system, no mixing needed
  • Will not cure without heating
  • Thermally conductive, electrically isolating
  • Paste consistency, but easy to dispense from a syringe

Information provided by Master Bond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.76 g/cc1.76 g/cc
Solids Content 100 %100 %
Viscosity 35000 - 95000 cP35000 - 95000 cPThixotropic paste
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 75 - 8575 - 85
Tensile Strength 13.8 - 20.7 MPa2000 - 3000 psi
Adhesive Bond Strength 3.45 - 4.14 MPa500 - 600 psiTensile lap shear, Al to Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.720 - 1.44 W/m-K5.00 - 10.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 177 °C350 °F
Minimum Service Temperature, Air -73.3 °C-100 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 120 - 180 min
@Temperature 85.0 °C
2.00 - 3.00 hour
@Temperature 185 °F
Shelf Life 3.00 - 6.00 Month3.00 - 6.00 MonthRefrigerated, in original, unopened containers
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMASTM5937 / 306826

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.