MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Osterman & Co Osterlene® LD070A LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product Description: LD070 is designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make this resin an ideal choice or bags used to package chemicals, agricultural and construction materials. LD070 has been designed for excellent processability, bubble stability and good heat sealing over a wide range of extrusion conditions. This resin is also well suited for shrink film applications.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America
Additive: Slip: No
Features: Excellent Processability; Good heat Seal; High Impact
Uses: Agricultural Applications; Construction Applications; Film; Heavy-duty Bags; Packaging
Processing Method: Extrusion

Information provided by Osterman & Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.921 g/cc0.0333 lb/in³ASTM D792
Melt Flow 0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 200 %200 %ASTM D882
Film Elongation at Break, TD 800 %800 %ASTM D882
Secant Modulus, MD 0.221 GPa32.0 ksiASTM D882
Secant Modulus, TD 0.276 GPa40.0 ksiASTM D882
Film Tensile Strength at Break, MD 33.1 MPa4800 psiASTM D882
Film Tensile Strength at Break, TD 21.4 MPa3100 psiASTM D882

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

POSTER060 / 267642

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.