MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Momentive Performance Materials RTV658 Low Volatile Silicone Adhesive Sealant, White, Mixed  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: RTV658 low volatile silicone adhesive sealant is a two component, thixotropic heat-curing silicone adhesive sealant that has a very long catalyzed work life at room temperature, but cures very quickly at elevated temperatures to a durable silicone rubber. It has a very high application rate to facilitate high volume robotic dispensing, but has sufficient thixotropy to avoid `sagging` in the uncured state.

RTV658 low volatile silicone adhesive sealant has been found useful for applications sensitive to the potential for silicone volatility. It achieves extremely low volatile and extractable levels without the need for a post-cure bake. Offering primerless adhesion to a wide range of substrates, it has been found useful for many types of applications, including formed-in-place gasketing.

Mechanical properties for specimen cured 1 hour at 150°C, mixed 10:1..

Key Performance Properties:

  • Low volatile and extractable levels
  • Long catalyzed pot-life at room temperature
  • Very fast cure at elevated temperatures
  • Primerless adhesion to many types of substrates
  • Excellent dielectric properties
  • Outstanding properties for robotic dispensing
  • Extended operating temperature performance

GE Silicones became a part of Momentive Performance Materials in 2006.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.17 g/cc1.17 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040
Tensile Strength, Ultimate 4.48 MPa650 psi
Elongation at Break 275 %275 %
100% Modulus 1.31 MPa
@Strain 100 %
190 psi
@Strain 100 %
200% Modulus 3.10 MPa
@Strain 200 %
450 psi
@Strain 200 %
Adhesive Bond Strength 1.03 MPa149 psiLap shear, aluminum to aluminum
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cm
Dielectric Strength 19.69 kV/mm500.1 kV/in
 
Descriptive Properties
Catalyzed Work Life>48 hours
ColorWhite
Flow0.2 inches
Mix Ratio10:1
Volatility<0.1%

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Momentive Performance Materials RTV658A Low Volatile Silicone Adhesive Sealant Component, White
Momentive Performance Materials RTV6702 One-Component,  Modified Alkoxy Adhesive Sealant, White
Momentive Performance Materials RTV658B Low Volatile Silicone Adhesive Sealant Component, Clear

PGESIL050 / 41041

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.