MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay Thornel® Graphite Cloth
Categories: Carbon; Carbon Fiber/Carbon Fibre; Graphite; Other Engineering Material; Composite Fibers

Material Notes: Carbon and graphite cloths, consisting entirely of flexible filaments, are produced by pyrolysis of rayon cloth at high temperatures to yield products with a high degree of purity. The cloth flexibility results from the very small filament diameter. These are fair conductors of electricity. At room temperature the volume resistivity of graphite cloth is about 40 times that of "Nichrome" wire. Graphite cloth resistance decreases with temperature, reaching half of the room temperature value at 1315°C.

99.9% carbon assay, 8.9 µm filament diameter

Solvay has acquired the Thornel product line as a part of the Cytec purchase.

Key Words: Carbon Fibre
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccCloth 1.42 g/cc per He measurement
Specific Surface Area 1.0 m²/gCloth
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 103 MPa
Tensile Modulus 13.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00600 ohm-cmor 0.39 ohm/sq (W) or 0.53 ohm/sq (F)
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 10.0 W/m-K
Maximum Service Temperature, Air 266 °C1% weight loss in 10,000 hours at 266°C.
 360 °C1% weight loss in 100 hours at 360°C
 493 °CShort term (1% weight loss in 1.0 hours)
Maximum Service Temperature, Inert 3650 °CSublimation temperature. Graphite cloth is stable in vacuum and inert atmospheres approaching this temperature.
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.90

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay Thornel® Mat VMA Carbon Fiber
Solvay Thornel® T-300 1K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Solvay Thornel® P-25 2K Carbon Fiber, Pitch Precursor
Solvay Thornel® T-300 3K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Toho Tenax Besfight® G30-400 1K HTA-7W EP01 Continuous Filament Carbon Fiber

ETHORT / 6101

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.