Exceed™ performance PE polymers Used to formulate a wide range of film structures offering superior mechanical performance for highly demanding end-use applications. Exceed 1023MJ is an ethylene 1-hexene copolymer. Films made from 1023MJ have outstanding tensile, impact strength, and puncture. These superior strength properties, along with excellent drawability, makes this a very versatile packaging film resin. TnPP is not intentionally added to Exceed 1023MJ. Availability: North America. Additive: Antiblock: 4500 ppm, processing aid: yes, slip: no, thermal stabilizer: yes. Applications: bag in box, form fill and seal packaging, packaging films, barrier food packaging, heavy duty bags, premium trash bags, blown film, multilayer packaging, stand up pouches. Information provided by ExxonMobil. |