MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SEKISUI SPI KYDEX® 6200 LTR Thermoplastic  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes: SMP800C compliant sheet for mass transit applications

KYDEX° 6200 LTR is formulated for mass transit interior applications where SMP800C compliance is required.

KYDEX® 6200 LTR is the next generation in our line of high performance thermoplastic sheet products for rail and bus interiors. It is a cost effective alternative to FRP due to its greater ease of fabrication. This product meets the recommended fire safety practices of both the Federal Transit Administration (FTA) and the Federal Rail Administration (FRA) for smoke emission and flammability when tested as per ASTM E662 and ASTM E162.

Suggested Applications:

  • Seatbacks
  • Bulkhead Components
  • Window Reveal
  • Ceiling Components

Features:

  • Specifically designed for mass transit industries
  • Compliant with SMP800C
  • Meets flamespread and smoke density requirements for mass transit
  • Excellent formability and fabrication quality
  • Good definition
  • Allows for tight tolerance
  • Easy trimming

Values based upon 3.175 mm (0.125 in) sheet unless otherwise specified.

Information provided by Sekisui Polymer Innovations

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.58 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 78ASTM D785
Tensile Strength 23.4 MPaASTM D638
Tensile Modulus 2261 MPaASTM D638
Flexural Strength 42.6 MPaASTM D790
Flexural Modulus 2710 MPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 180 °CAnnealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 160 °FAnnealed; ASTM D648
 
Descriptive Properties
FlammabilityPassASTM E162; Radiant Panel Is; tested by an accredited third party lab
 PassASTM E662; Smoke Generation, Ds @ 4.0 minutes; tested by an accredited third party lab
 PassSMP 800C; Toxicity Requirements; tested by an accredited third party lab

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SEKISUI SPI KYDEX® 430 ABS/PVC
SEKISUI SPI KYDEX® 410 ABS/PVC
SEKISUI SPI KYDEX® T Thermoplastic
SEKISUI SPI KYDEX® 6513 Thermoplastic
SEKISUI SPI KYDEX® FST2 Thermoplastic

PSEKIS039 / 185864

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.