MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

NuSil EPM-2461 Silicone, Static Dissipative
Categories: Polymer; Thermoset; Silicone

Material Notes: General Purpose: Static Dissapative

Comments: Carbon black filled for EMI shielding applications

Cure system: Platinum

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 100000 cP100000 cPB
 1.25e+6 cP1.25e+6 cPA
 
Chemical PropertiesMetricEnglishComments
Ionic Impurities - Na (Sodium) <= 6.0 ppm<= 6.0 ppm
Ionic Impurities - K (Potassium) <= 1.0 ppm<= 1.0 ppm
Ionic Impurities - Cl (Chloride) <= 5.0 ppm<= 5.0 ppm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3030
Tensile Strength at Break 3.80 MPa551 psi
Elongation at Break 400 %400 %
Tear Strength 5.26 kN/m30.0 pli
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 900 ohm-cm900 ohm-cmASTM D257
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Working Life 60.0 min
@Temperature 25.0 °C
60.0 min
@Temperature 77.0 °F
 
Descriptive Properties
ColorBlack
Mix Ratio1:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CoorsTek StatSafe™ ADC Static Dissipative Alumina
NuSil CV-2644 Silicone, Conductive/Static Dissipative
NuSil CV2-2646 Silicone, Conductive/Static Dissipative
Westlake Plastics Zelux® SD-P Polycarbonate (static dissipative)
RTP Company RTP 2099 X 138791 PC/PBT; Permanently Static Dissipative - ESD Protection

PNUSIL255 / 141979

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.